75. Leszczynska A, Njuguna J, Pielichowski K, Banerjee JR (2007) Polymer/montmorillonite
nanocomposites with improved thermal properties Part I. Factors influencing thermal stabil-
ity and mechanisms of thermal stability improvement. Thermochim Acta 453:75-96
76. Leszczynska A, Njuguna J, Pielichowski K, Banerjee JR (2007) Polymer/montmorillonite
nanocomposites with improved thermal properties Part II. Thermal stability of montmoril-
lonite nanocomposites based on different polymeric matrixes. Thermochim Acta 454:1-22
77. Pavlidou S, Papaspyrides CD (2008) A review on polymer-layered silicate nanocomposites.
Progr Polym Sci 33:1119-1198
78. Chrissafis K, Bikiaris D (2011) Can nanoparticles really enhance thermal stability of poly-
mers? Part I: an overview on thermal decomposition of addition polymers. Thermochim Acta
523:1-24
79. Bikiaris D (2011) Can nanoparticles really enhance thermal stability of polymers? Part II:
an overview on thermal decomposition of polycondensation polymers. Thermochim Acta
523:25-45
80. Vyazovkin S, Dranca I, Fan X, Advincula R (2004) Degradation and relaxation kinetics of
polystyrene-clay nanocomposite prepared by surface initiated polymerization. J Phys Chem
B 108:11672-11679
81. Chen K, Wilkie CA, Vyazovkin S (2007) Nano-confinement revealed in degradation and
relaxation studies of two structurally different polystyrene-clay systems. J Phys Chem B
111:12685-12692
82. Yancey B, Vyazovkin S (2014) Venturing into kinetics and mechanism of nanoconfined sol-
id-state reactions: trimerization of sodium dicyanamide in nanopores. Phys Chem Chem Phys
16:11409-11416
83. Li Q, Simon SL (2008) Curing of bisphenol M dicyanate ester under nanoscale constraint.
Macromolecules 41:1310-1317
84. Koh YP, Simon SL (2011) Kinetic study of trimerization of monocyanate ester in nanopores.
J Phys Chem B 115:925-932
85. Jang BN, Wilkie CA (2005) The thermal degradation of polystyrene nanocomposite. Polymer
46:2933-2942
86. Chen K, Susner MA, Vyazovkin S (2005) Effect of the brush structure on the segradation
mechanism of polystyrene-clay nanocomposite. Macromol Rapid Commun 26:690-695
87. Chen K, Vyazovkin S (2006) Mechanistic differences in degradation of polystyrene and poly-
styrene-clay nanocomposite: thermal and thermo-oxidative degradation. Macromol Chem
Phys 207:587-595
88. Sanchez-Jimenez PE, Perez-Maqueda LA, Perejon A, Criado JM (2012) Nanoclay nucleation
effect in the thermal stabilization of a polymer nanocomposite: a kinetic mechanism change.
J Phys Chem C 116:11797-11807
89. Chen K, Harris K, Vyazovkin S (2007) Tacticity as a factor contributing to the thermal stabil-
ity of polystyrene. Macromol Chem Phys 208:2525-2532
90. Sanchez-Jimenez PE, Perez-Maqueda LA, Perejon A, Criado JM (2010) A new model for
the kinetic analysis of thermal degradation of polymers driven by random scission. Polym
Degrad Stabil 95:733-739
91. Simha R, Wall LA (1952) Kinetics of chain depolymerization. J Phys Chem 56:707-715
92. Young DA (1966) Decomposition of solids. Pergamon, Oxford
93. Brown ME, Dollimore D, Galwey AK (1980) Reactions in the solid state. Elsevier, Amster-
dam
94. Glawey AK, Brown ME (1999) Thermal decomposition of ionic solids. Elsevier, Amsterdam
95. Stern KH (2000) High temperature properties and thermal decomposition of inorganic salts
with oxyanions. CRC Press, Boca Raton
96. MacDonald JY, Hinshelwood CN (1925) The formation and growth of silver nuclei in the
decomposition of silver oxalate. J Chem Soc 128:2764-2771
97.
Khawam A, Flanagan DR (2006) Solid-state kinetic models: basics and mathematical funda-
mentals. J Phys Chem B 110:17315-17328