Fig. 8.28
Higher
magnification of the image of
the metal/ceramic interface
from Fig.
8.27,
showing that
the Ti/Pt/SiO
2
interface is
fractured. (
J. Ayache,
S. Collin CNRS-CSNSM
Orsay
)
Fig. 8.29
Bright-field TEM
image of a cross section of
the multilayer material
prepared using ionic thinning,
dimpling with liquid nitrogen.
This image shows a selective
abrasion of the interfaces at
low magnification (
J. Ayache,
Cheng Y. Song NCEM,
Berkeley
)