Figure 6.8 Weathering of unstabilized LDPE films ( open symbols ) and
enhanced photodegradable ECO copolymer ( filled symbols ) exposed
outdoors in Miami, FL.
Table 6.2 Location-dependent Enhancement in
Photodegradation Obtained Using ECO Copolymer in Place of
LDPE Laminate of Same Thickness (Andrady et al., 1993a)
Location of
exposure
Degradable plastic
ECO ( B × 10 3 ) days −1
Control plastic LDPE
( B × 10 3 ) days −1
B */ B
Cedar Knolls,
NJ
52
9.5
5.5
Chicago, IL
87
4.3
20
Miami, FL
69
14
4.9
Seattle, WA
40
4.2
9.5
Whitman, AZ 257
25
10
 
 