FIGURE 4.19
Morphological aspect of Filtek Supreme XT after 2 years of simulated
wear (8,000). Small cracks and filler debonding can be observed.
Source: Braun and Oshima (2008).
FIGURE 4.20
Morphological aspect of Filtek Supreme XT after 4 years of simulated
wear (8,000).
Source: Braun and Oshima (2008).
 