Figure 15.5. Time series of photographs showing recovery of a shape-memory tube. a-f, Start
to fi nish of the process; total time, 10s at 50 °C. The tube was made of a poly(
-caprolactone)
dimethacrylate polymer network (the M n of the network's switching segments was 104) that
had been programmed to form a fl at helix. Adopted from [3].
ε
stimulus in nervous system development and improving spinal cord injury, and
the complexities involved in designing such studies have been emphasized.
The chapter by Chandra P. Sharma and K. Kaladhar demonstrates the upcom-
ing importance of cell mimetic monolayer and their blood biocompatibility. The
authors have included various approaches to design monolayer fi lms on surface
including the fundamentals involved in monolayer deposition on any surface. The
effect of changing the composition of the lipid (mimicking the cell bilayer) mono-
 