Biomedical Engineering Reference
In-Depth Information
Figure 5.14 Magnified views of
the regions in Fig. 5.13 :(a)
Fracture initiation site showing
coalesced voids; (b) further
magnified view showing the
ductile nature of the coalesced
voids; (c) patchwork
morphology indicative of
crazing; (d) fast fracture region.
Courtesy of Ref. [38] .
(a)
(c)
(b)
(d)
Figure 5.15 Experimental data and regression curves based on the Basquin relationship for three notch geometries of
PEEK 450G tested in fatigue. Courtesy of Ref. [39] .
Figure 5.16 Representative fracture surfaces of notched PEEK 450G fatigue specimens. Courtesy of Ref. [39] .