150. Laudise, R. A. 1970. The Growth of Single Crystals , 278-281. Englewood Cliffs, NJ: Prentice-
Hall.
151. Rabenau, A. 1985. The role of hydrothermal synthesis in preparative chemistry. Angew. Chem.
(Engl. Ed.) 24:1026-1040.
152. Lobachev, A. N. 1973. Crystallization Process under Hydrothermal Conditions , 1-255. New York,
NY: Consultants Bureau.
153. Roy, R. 1994. Acceleration the kinetics of low-temperature inorganic syntheses. J. Solid State
Chem . 111:11-17.
154. Byrappa, K. 1992. Hydrothermal Growth of Crystals , 1-365. Oxford, UK: Pergamon Press.
155. Roy, D. M., and S. K. Linnehan. 1974. Hydroxyapatite formed from coral skeletal carbonate by
hydrothermal exchange. Nature 247:220-222.
156. Ito, A., Nakamura, S., and H. Aoki, et al. 1996. Hydrothermal growth of carbonate-containing
hydroxyapatite single crystals. J. Cryst. Growth 163:311-317.
157. Ito, A., Teraoka, K., Tsutsumi, S., and T. Tateishi. 1996. Single crystal hydroxyapatite: Preparation,
composition and mechanical properties. Bioceramics 9:189-192.
158. LeGeros, R. Z. 1991. Calcium Phosphates in Oral Biology and Medicine Vol. 15 . Basel: S. Karger.
159. LeGeros, R. Z. 1967. Crystallographic studies of the carbonate substitution in the apatite struc-
ture. PhD thesis, New York University.
160. Kokubo, T., Kim, H. M., and M. Kawashita. 2003. Novel bioactive materials with different
mechanical properties. Biomaterials 24:2161-2175.
161. Yamasaki, N., Yanagisawa, K., Nishioka, M., and S. Kanahara. 1986. Hydrothermal hot-pressing
method: Apparatus and application. J. Mater. Sci. Lett. 5:355-356.
162. Onoki, T., Hosoi, K., and T. Hashida. 2003. Joining hydroxyapatite ceramics and titanium alloys
by hydrothermal method. Key Eng. Mater. 240-242:571-574.
163. Onoki, T. Higashi, T., and X. Wang et al. 2009. Interface structure between Ti-based bulk metal-
lic glasses and hydroxyapatite ceramics jointed by hydrothermal techniques. Mater. Trans.
50[6]:1308-1312.
164. Monma, H., and T. Kamiya. 1987. Preparation of hydroxyapatite by the hydrolysis of brushite.
J. Mater. Sci. 22:4247-4250.
165. Li, J., and T. Hashida. 2007. Preparation of hydroxyapatite ceramics by hydrothermal hot-
pressing method at 300°C. J. Mater. Sci . 42:5013-5019.
166. Onoki, T., Hosoi, K., and T. Hashida et al. 2008. Effects of titanium surface modifications on
bonding behavior of hydroxyapatite ceramics and titanium by hydrothermal hot-pressing.
Mater. Sci. Eng. C 28:207-212.
167. Chang, C., Huang, J., Xia, J., and C. Ding. 1999. Study on crystallization kinetics of plasma
sprayed hydroxyapatite coating. Ceram. Int . 25:479-483.
168. Roeder, R. K., Converse, G. L., Leng, H., and W. Yue. 2006. Kinetics effects on hydroxyapatite whis-
kers synthesized by the chelate decomposition method. J. Am. Ceram. Soc . 89[7]:2096-2104.
169. Campos, A. L., Silva, N. T., Melo, F. C. L., Oliverira, M. A. S., and G. P. Thim. 2002. Crystallization
kinetics of orthorhombic mullite from diphasic. J. Non-Cryst. Solids 304:19-24.
170. Huang, L. Y., Xu, K. W., and J. Lu. 2000. A study of the process and kinetics of electrochemical
deposition and the hydrothermal synthesis of hydroxyapatite coatings. J. Mater. Sci.: Mater.
Med . 11:667-673.
171. Yang, C. W., and T. S. Lui. 2009. Kinetics of hydrothermal crystallization under saturated
steam pressure and the self-healing effect by nanocrystallite for hydroxyapatite coatings. Acta
Biomater . 5:2728-2737.
172. Tong, W., Chen, J., Cao, Y., Lu, L., Feng, J., and X. Zhang. 1997. Effect of water vapor pressure
and temperature on the amorphous-to-crystalline HA conversion during heat treatment of HA
coatings. J. Biomed. Mater. Res . 36:242-245.
173. Zeng, H., and W. R. Lacefield. 2001. XPS, EDX and FTIR analysis of pulsed laser deposited
calcium phosphate bioceramic coatings: The effects of various process parameters. Biomaterials