reaction, the presence of silica and alumina in PCCRs significantly contributed
for the formation of new crystallite phases leading to detoxify the toxic
substance in the jarosite waste.
Actual Components:
X 1 =A: Jarosite = 515 g
X 2 = B: Clay = 282.5 g
X 3 = C: PCCRs = 202.5 g
Figure 11. Response trace plot for compressive strength of s/s sintered Jarosite waste-
clay-PCCRs composite bricks.
Figure 12. Response contour plot for compressive strength of s/s sintered Jarosite
waste -clay PCCRs composite bricks.