Figure 7.7 Arsenic deposition on a Pt(775) electrode from 1 mMAs 2 O 3 รพ 0.1 M H 2 SO 4
solution. Sweep rate: 50 mV/s.
Figure 7.8 Different stages in Se and S deposition on a Pt(775) electrode in 0.5 M H 2 SO 4
solution containing 5 mM SeO 2 and Na 2 S, respectively. The dashed line is the first scan, the