Figure 5.38
C in 1 atm of O 2 , using the
''cold insertion'' (CI) oxidation procedure. At each temperature oxidation is greater for
cold-worked (C.W.) Ni (broken lines) than annealed Ni (solid lines) [Ref. 64].
Oxidation curves for Ni from 700 to 1270
°