Fig. 2. SEM images (X1000) showing the fractured surface between the composite resin and
dentin side. The fractured bonded surface of dentin by the single bond adhesive treatment
as a result of the shear bond strength test followed by 37% phosphoric acid etching (A), and
1.4 W of power intensity irradiation followed by a Single bond procedure (B), and 2.25 W of
power intensity irradiation followed by a Single bond procedure (C) were evaluated by
SEM. The fractured bonded surface of the dentin by Clearfil SE bond adhesive treatment as
a result of the shear bond strength test followed by 37% phosphoric acid etching (D), and 1.4
W of power intensity irradiation followed by the SE bond procedure (E), and 2.25 W of
power intensity irradiation followed by the SE bond procedure (F) were evaluated by SEM.